Dear Expert,

Can you give some information about P number of X12CrMoWVNbN-10-1-1 with reference?

Thanks in advance.

Ranendra Chakraborty 

sridhar cn

unread,
Apr 16, 2026, 11:19:27 PMApr 16
to material...@googlegroups.com

X12CrMoWVNbN-10-1-1   (EN No. 1.4906) is a high-alloy martensitic creep-resistant steel used in turbines and 

high-temperature service. It is not listed in ASME Sec IX QW/QB-422; hence it is treated as an unassigned material. 

Based on composition (10% Cr-Mo-W-V-Nb), it is metallurgically comparable to P91/P92 steels and aligns closest 

with P-No. 5C. Under ISO15608 grouping this material falls under Group 10/Cr-Mo-V creep resistance steels.

Sridhar.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANGGva%2BObPxBiA1Ye7jhzPE_KDkA6%3DF1zoB4B_OWA1WxgdHJ8Q%40mail.gmail.com.

Sankaran Sp

unread,
Apr 21, 2026, 12:24:21 PMApr 21
to material...@googlegroups.com
Dear friends,
below said material  is belongs to forging material.  

X12CrMoWVNbN-10-1-1   (EN No. 1.4906), this is not P91/F91 type steel. 

This is F92/P92 type forging or pipe material is under P no of 15E as per ASME sec VIII Div 1  
 