Dear Expert

Welding application: compressor piping
Process: GMAW 1.2mm ER70S-6
Welding issue: silicone contamination after welding

How can I reduce the silicon content?
Any special method or consumable which can solve this issue?

Kindly advice.

Pravin Poornachandran
Singapore

Sent from my iPhone

Ahmad el-sharkawy

unread,
Jun 17, 2015, 3:33:00 AM6/17/15
to material...@googlegroups.com
can you send chemical composition of piping and welding electrode also? and tell us what is problems and percent of silicon at weld metal?


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7941CE40-4030-4247-AABE-EB015A292649%40gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
WITH MY BEST WISHES

AHMED ELSHARKAWY
QA/QC ENGINEER
DIPLOMA DEGREE IN WELDING ENGINEERING.
CERTIFIED WELDING INSPECTOR " CWI " 14072901.
ASNT LEVEL II " RT&VT&UT&PT&MT"
IRECA CERTIFIED LEAD EDITOR ISO 9001/2008.
PREPARING MASTER DEGREE IN WELDING ENGINEERING.

Kannayeram Gnanapandithan

unread,
Jun 17, 2015, 4:49:48 AM6/17/15
to materials-welding
change over to another consumable manufacture

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Wed, Jun 17, 2015 at 1:58 PM, Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:
is it like a slag?? at random

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

meisam shokri arfaei

unread,
Jun 17, 2015, 9:59:22 AM6/17/15
to material...@googlegroups.com
In the first step you have to investigate the root cause of the high Si content. Is it just slight percentage from the base material or consumable or etc, or is it higher percentage caused from grinding remain or etc.


For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ISA-ISTS - Metallurgy Lab. Manager
ASNT NDT Level III
International Welding Engineer





Anup N K E

unread,
Jun 17, 2015, 12:14:55 PM6/17/15
to material...@googlegroups.com

Replace ER 70S-6 with ER70S- 3 GMAW filler wire. Silicon content is 0.45 % to 0.75% for ER70S-3  and 0.8 % to 1.15 % for ER 70S- 6.

This is as per Aramco recommendation.

Regards,

Anup

Srini Vasan

unread,
Jun 19, 2015, 11:06:00 AM6/19/15
to material...@googlegroups.com
Guys I face high silicon content in ER70S-3 with high rejection repair rate,after changing of ER70S-6 we reduce repair rate.better purchase different manufacturer,and verify purging gas purity.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJsQutbzSCJZTnrU3Q3Rzh0%3DjKtubQx_bkHLEh2SUgHJWBdz1A%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.


--
With Best & Regards

N.Srinivas,
Welding Inspector,
0561198050,0537812787
Al-Khobar.

Reply all
Reply to author
Forward
0 new messages