Dear Mr. Pandiyanplease refer below attachment
On Thu, Feb 17, 2022 at 4:17 PM Maruthu Pandian <maruthupa...@gmail.com> wrote:
Dear allI have one Doubt regarding the reinforcement pad which is designed by B31.3. I get all the clearances from the design team. But I just wonder if the pad will be cut by two pieces lateral to run pipe and merged on the location.My Client told me that the case is code wise ok.So now I have to Submit my WMS for that work.In B31.3 there is nothing about it. So please generals if you have any about that ... Please share with me.Herewith I attached the Photo also--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ3bEeXbpLZnKVLYEwH0NpKkP6Het6i6raC2EwEHSBYg_049Kg%40mail.gmail.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHwwqE9X%3DqxyfsOB1YCZwSkMPM1_3K9FiL1q5RCK-MjMZdbRdw%40mail.gmail.com.
Dear Mr. Pandiyanplease refer below attachment
On Thu, Feb 17, 2022 at 4:17 PM Maruthu Pandian <maruthupa...@gmail.com> wrote:
Dear allI have one Doubt regarding the reinforcement pad which is designed by B31.3. I get all the clearances from the design team. But I just wonder if the pad will be cut by two pieces lateral to run pipe and merged on the location.My Client told me that the case is code wise ok.So now I have to Submit my WMS for that work.
In B31.3 there is nothing about it. So please generals if you have any about that ... Please share with me.Herewith I attached the Photo also
--<WhatsApp Image 2022-02-17 at 10.53.43 AM.jpeg>==============Thanks & RegardsSUNGDO ENGINEERINGMARUTHU PANDIAN.NEngineer (Piping & Quality Control)Polimery Police PDH/PP Project, PolandMob +48571461164
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJ3bEeXbpLZnKVLYEwH0NpKkP6Het6i6raC2EwEHSBYg_049Kg%40mail.gmail.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHwwqE9X%3DqxyfsOB1YCZwSkMPM1_3K9FiL1q5RCK-MjMZdbRdw%40mail.gmail.com.
<Pad.pdf>