Dear experts,

Kindly advise if any code or standard specify to use pressure chart recorder for piping spools hydrotest.

The client asking to use it although it is not mentioned in the approved procedure/ITP.

Please advise.

Thanks,
Mahmood

Tajuddin Mohammed

unread,
Feb 16, 2026, 2:43:26 AMFeb 16
to material...@googlegroups.com
Pressure chart recorder is normallly used in buried pipelines morethan 10% of its length

Thanks & Regards
Mohammed Tajuddin
WELDING INSPECTOR CSWIP 3.1
Contact  0530833486
JUBAIL



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANV5n6ja_XKiu8F5BBpa0vK0hW-CeJ%2BgttfPDuecYvdJfmUz%2Bw%40mail.gmail.com.

venkateswara reddy Desireddy

unread,
Feb 16, 2026, 4:18:41 AMFeb 16
to material...@googlegroups.com
If you have agreement with enduser then recorded mandatory.As per ASME codes recorder not mandatory.

DOMINIC V.K

unread,
Feb 19, 2026, 12:51:50 PMFeb 19
to material...@googlegroups.com

It depends on the project requirements. In our current project, we are using a hydrotest pressure chart recorder for both above-ground and underground lines, as per the specification requirements.

If the company requires it, this should be clearly stated in the agreement and hydrotest specification, because it is not only for recording purposes but also involves additional cost.

Please convey this to your Quality Management team; they will decide as per the agreement.  

Best regards,
Dominic V




Jay Poojary

unread,
Feb 19, 2026, 1:03:31 PMFeb 19
to material...@googlegroups.com
Dear Experts,
Chart recorder are used only to keep evidence records for future reference. If it is not mentioned in client spec & in the approved procedure, you may strongly take up with client to avoid it.

cordially,
Jay Poojary

pradip kumar Sil

unread,
Mar 19, 2026, 3:07:30 AMMar 19
to material...@googlegroups.com
Hi,
It is not mandatory as per code. Pls check your contract document if there is any client requirement.

Mohd Siraj

unread,
Jun 29, 2026, 9:08:35 AMJun 29
to Materials & Welding
not require ,if can prove with guage and hourly monitoring guage reading sheet by QC. try digital guage.