PMI for ASTM A105 Flanges

280 views
Skip to first unread message

Babur Khan

unread,
Apr 21, 2021, 11:42:47 PM4/21/21
to material...@googlegroups.com
Dear Experts,
One of our contractor purposed PMI for ASTM A105 Flanges due to lake of inspection documents.
As my understanding PMI is suitable for HSLAS,
SS and DSS. For carbon Steel we can check if there is something happened im change of welding consumables for welding.
Please share your experience.

Babur Khan Lashari

Sent from my iPhone

Muhammad Babur Khan
Sent from my iPhone

Vishnu Nandan

unread,
Apr 22, 2021, 5:32:17 AM4/22/21
to material...@googlegroups.com
Hi Babur,



Positive material identification is performed using either of the two techniques below:

  • X-ray Fluorescence (XRF) analyser: This is the most common method and the portability of the hand-held equipment allows Intertek to perform PMI on-site at our customers’ premises. The device scans the metal material and identifies its key elements. However, it cannot detect carbon and some lighter elements and is not suitable for identification of pure carbon steel materials.
  • Optical Emission Spectroscopy (OES): This method can detect almost all types of elements including carbon and lighter elements and carbon steel. Although not as portable as XRF analysers, the equipment can be transported to sites and used at high elevations with proper lifting arrangements.
VISHNU  NANDAN
Mechanical  Engineer


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/F2094BAB-A558-456E-9910-FD7962768B98%40gmail.com.

james gerald

unread,
Apr 22, 2021, 5:32:17 AM4/22/21
to material...@googlegroups.com
I suppose this issue may be due to non-availability of MTC or due to Heat Number Traceability. If this is the case, then PMI by suitable methods to reveal the chemical composition of the Flange an option

Thanks & Regards

J.Gerald Jayakumar




--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

james gerald

unread,
Apr 22, 2021, 9:39:40 AM4/22/21
to material...@googlegroups.com
Just to add, the term PMI may not be apt as PMI is used to determine only the Major alloying elements but in this case the Chemical composition as per ASTM A 105 checked has to be checked and evaluated.

Thanks & Regards

J.Gerald Jayakumar


On Thursday, 22 April, 2021, 09:12:44 am IST, Babur Khan <mbabu...@gmail.com> wrote:


Ramin Kondori

unread,
Apr 22, 2021, 11:24:29 PM4/22/21
to material...@googlegroups.com
PMI will not work in this case...
You have to take samples for mechanical testing...
Tensile and Impact tests are essential for A105...

Regards
Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Vinay Thattey

unread,
Apr 25, 2021, 11:19:48 PM4/25/21
to material...@googlegroups.com
Dear Khan ;

PMI can be opted but it's not an alternative to chemical testing .  Yor statement " For carbon Steel we can check if there is something happened im change of welding consumables for welding" is not clear ...Can you specify . Well .What about physical properties ?

Chaitanya Purohit

unread,
Apr 25, 2021, 11:19:48 PM4/25/21
to material...@googlegroups.com
In case of MTC non Availability or traceability chemical, mechanical and heat treatment condition to be proved. 

All test required by A105 and some additional test for heat treatment condition to be carried out. 