Dear Experts,
In one of our job 51 mm. thk. SB 171 UNS C46400 plate is going to be used in exchanger for which El.% actual observed 19.5 in check testing against requirement of 35% min. as per code. Chemical composition meets the code requirements.
Please suggest me the proper annealing temp. incl. heating rate, holding temp. and time, cooling rate for re heat treat the plate to meet the Elongation requirement as per code.
Awaiting for your prompt response at the earliest.
Have a good day.
Thanks & regrads,
C. R. GANDHI
(Manager- Q. A./ Q.C.) |
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
| Hi! Such heat treatment should be recomended by Plate mfgr so please ask them This is to retain all other mech properties Regards Hegde P.b. --- On Sat, 9/3/13, sonu shahu <shahu...@gmail.com> wrote: |
|