A piping spool is to be fabricated.
Construction code: ASME B 31.3

Service LPG liquid
MDMT : minus 45 degree Celsius

Client spec calls for impact requirements. 

Pipe MOC is A 333 grade 6; Size 2 inch schedule 80 and 3 inch schedule 40.

My question is are these two thicknesses of 5.54mm and 5.49mm exempt from impact testing as per B 31.3 Fig. 323.2.2A curves ??

Please provide B 31.3 code reference. 

Regards

Prem Nautiyal
9769316004


Sent from Samsung Mobile

Hafiz Ali Alvi

unread,
Jun 15, 2016, 11:14:39 PM6/15/16
to material...@googlegroups.com
Impact testing is mandatory requirement for A333.

Hafiz Ali Alvi

Sent from my iPhone
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/w307dtxxgn6ng9cqo11020e4.1466005983348%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

MW

unread,
Jun 17, 2016, 12:20:05 AM6/17/16
to Materials & Welding, prem_na...@yahoo.com
base metal can be exempted, unless your project specification says so. refer Table A-1, however welding procedure impact tests are required
A listed material may be used at any temperature not lower than the minimum shown in Table A-1, provided that the base metal, weld deposits, and heataffected zone (HAZ) are qualified as required by the applicable entry in Column A of Table 323.2.2.