separate PQR for Fillet position like3F,4F or 2F required or not?

57 views
Skip to first unread message

hasin shaikh

unread,
Dec 8, 2015, 12:10:05 AM12/8/15
to material...@googlegroups.com
Dear Experts

As per Sec.IX if I have done PQR for 3G & 2G position for storage Tank welding then  is it required to established or perform any other separate  PQR for Fillet position like3F,4F or 2F

--
*With Regards
Shaikh.Hasin
Email: hasin....@gmail.com
Mobile: +91-9924562942*


Mohd Azam

unread,
Dec 8, 2015, 12:23:32 AM12/8/15
to material...@googlegroups.com
No

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMu5BBA97U0hR2W3quB-hTJD7%3D%2Bfh0Yh-PXptdG4jS3V3ZQVWw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

george....@gr.bureauveritas.com

unread,
Dec 8, 2015, 2:54:23 AM12/8/15
to Mohd Azam
In ASME IX position is not an essential variable for PQR

Sent from my BlackBerry 10 smartphone.
From: Mohd Azam
Sent: Τρίτη, 8 Δεκεμβρίου 2015 - 07:23
Subject: Re: [MW:23955] separate PQR for Fillet position like3F,4F or 2F required or not?


For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Kannayeram Gnanapandithan

unread,
Dec 8, 2015, 2:59:56 AM12/8/15
to material...@googlegroups.com

Is there any impact requirements, if not, u need not do again, if it is there then u have to do

george....@gr.bureauveritas.com

unread,
Dec 8, 2015, 4:36:46 AM12/8/15
to material...@googlegroups.com

to be more accurate, when impact test is a requirement and you change from a given position to the vertical uphill position.
If the PQR was done on a vertical uphill progression then you do not need a new PQR even when impact test is a requirement

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for Kannayeram Gnanapandithan ---08/12/2015 10:00:11---Is there any impact requirements, if not, u need nKannayeram Gnanapandithan ---08/12/2015 10:00:11---Is there any impact requirements, if not, u need not do again, if it is there then u have to do

.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAJzm4eNv9pcK5q_kt5yRx1yCAM8vMDSJRjJGyn6nuqUG3PTj1A%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Reply all
Reply to author
Forward
0 new messages