anyone have procedure for characterisation of pipe API 5L X60 
Such as the test that will be use are 
- tensile test 
- bending test 
- hardness test 
- impact test 
please i need it urgantly 

abdullah Alhiji

unread,
Mar 6, 2023, 7:47:33 AM3/6/23
to material...@googlegroups.com
Hi, You can use the following as guideline: 

  1. Tensile Test:
  • Cut a sample from the pipe according to ASTM E8/E8M.
  • Machine the sample according to the ASTM standard.
  • Perform a tensile test on the sample according to the ASTM standard.
  1. Bending Test:
  • Cut a sample from the pipe according to ASTM A370.
  • Machine the sample according to the ASTM standard.
  • Perform a bending test on the sample according to the ASTM standard.
  1. Hardness Test:
  • Cut a sample from the pipe according to ASTM E8/E8M.
  • Machine the sample according to the ASTM standard.
  • Perform a hardness test on the sample according to the ASTM standard.
  1. Impact Test:
  • Cut a sample from the pipe according to ASTM E23.
  • Machine the sample according to the ASTM standard.
  • Perform an impact test on the sample according to the ASTM standard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5225f762-78b6-4e12-828f-58bbac027fdfn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages