The flatolet is basically "olet" to be used on flat surface or on the very
large run sizes (where the difference of curvature becomes less and less
significant. As per bonney forge catalogue, the weldolet for run sizes
larger than 36" (DN 1800) will be considered as flatolet.

Please note that one needs to specify this in the purchase order whether
you require flatolet.

Hope to have clarified

Best regards,

Prasad




"Sreejith.Nair"
<fizzyshadow@gmai
l.com> To
Sent by: material...@googlegroups.com
materials-welding cc
@googlegroups.com
Subject
[MW:1639] flatolet
25/02/09 06:42 PM


Please respond to
materials-welding
@googlegroups.com







can anybody please explain what a flatolet is?? it would be a great help if
a picture of the same can be posted.



Save a tree...please don't print this e-mail unless you really need to.







Save a tree...please don't print this e-mail unless you really need to.

SENTHILKUMAR SWAMINATHAN

unread,
Feb 25, 2009, 10:58:57 AM2/25/09
to material...@googlegroups.com
Sreejith,
 
Olet which will be in Flat. Assy in plate etc.. Find attached fig.
 
Regards,
S.Senthilkumar

--- On Wed, 25/2/09, Sreejith.Nair <fizzy...@gmail.com> wrote:

Add more friends to your messenger and enjoy! Invite them now.
Untitled.pdf
Flatolet Low.pdf
Reply all
Reply to author
Forward
0 new messages