The picture below shows the internal pressure inside the tank of the pipe. Does it need to be radiographically tested according to Asme Sec VIII Div.1?

Screenshot_1.jpg

Pravin Kurade

unread,
Oct 9, 2022, 11:25:35 PM10/9/22
to material...@googlegroups.com
This will be considered as non pressure part and hence no need to conduct RT 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a698c2f0-0cb2-44cd-93f6-a15de0664398n%40googlegroups.com.
--
Pravinkumar kurade

Avanish Singh

unread,
Oct 9, 2022, 11:25:35 PM10/9/22
to material...@googlegroups.com
For Internal Pipe , Don't Need to do Radiography.

--

Sezgin Ckllı

unread,
Oct 10, 2022, 3:52:03 AM10/10/22
to Materials & Welding
Where can I find this explanation in Asme Sec.VII, can you explain this situation?

Thanks
10 Ekim 2022 Pazartesi tarihinde saat 06:25:35 UTC+3 itibarıyla Avanish Singh şunları yazdı:

G Gughan

unread,
Oct 11, 2022, 6:01:31 AM10/11/22
to material...@googlegroups.com
Dear Sezgin,

                  Please refer to UW-2 (-a) for welded tubes & pipes internal. It is not considered under any category of UW-3. I hope it is correct & will assist you.

Thanks,

Kind Regards,

G.Gughan


G Gughan

unread,
Oct 11, 2022, 6:05:32 AM10/11/22
to material...@googlegroups.com
Dear Sezgin,

                       There is an exemption for welded tubes & pipe internal under UW-2 (-a).

Thanks,

Kind Regards,

G.Gughan