Can we avoid PWHT for P No.5A to P No.1 , 10mm weld joint ?

90 views
Skip to first unread message

PARAI Reaction Channel

unread,
May 22, 2025, 8:24:36 AM5/22/25
to materials-welding@googlegroups com

Dear Sirs ,

 

We have a project with both shell and Reinforcement Pad materials SA516-70, 10 mm Thk ( P No.1 ) and the Nozzle is SA335-P22, 4 Sch 120 , 

11.1 mm ( P No.5A ) Thk.

 We already have a qualified WPS & PQR with 8mm GTAW and tested about 10 years ago by other welding engineer, for P No,.5A to P No.1 without PWHT and it was satisfactorily passed and we 

have used that WPS & PQR for the previous project 10 years ago and no 

issues found without PWHT.

 Now for the new project, we are going to use the same WPS and apply 

Preheat ( 204 to 250 Deg C ) as per the WPS for 10mm Shell Thk by 

multipass welding, refer to the below sketches.

image.png


image.png


So, i would like to confirm whether PWHT is mandatory as per UCS-56-4 ?

Can we avoid PWHT for this 10mm weld joint ?


Or Should we do buttering with ERNiCr-3 on P No.5A bevel and butt weld 

with same filler for this dissimilar joint to avoid PWHT after making new 

PQR with buttering?


Please confirm soon.


Thanks and Regards,

Saravanan Sornam,

ANSAN-Si,

S.Korea 

Raghuram Bathula

unread,
May 22, 2025, 8:26:19 AM5/22/25
to Materials-Welding
Why do you use P22 nozzles on CS?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2Biby3LDhuASFD6Sx3wD6mhOVKRXA8dsJCQcfO-yNsjhQ%40mail.gmail.com.

Vishwas Keskar

unread,
May 22, 2025, 10:23:11 AM5/22/25
to material...@googlegroups.com, Materials-Welding
Butt welds 
Acceptable 
Sent from my iPhone

On 22 May 2025, at 2:26 PM, Raghuram Bathula <raghura...@gmail.com> wrote:


Why do you use P22 nozzles on CS?

On Thu, 22 May 2025, 16:24 PARAI Reaction Channel, <sarava...@gmail.com> wrote:

Dear Sirs ,

 

We have a project with both shell and Reinforcement Pad materials SA516-70, 10 mm Thk ( P No.1 ) and the Nozzle is SA335-P22, 4 Sch 120 , 

11.1 mm ( P No.5A ) Thk.

 We already have a qualified WPS & PQR with 8mm GTAW and tested about 10 years ago by other welding engineer, for P No,.5A to P No.1 without PWHT and it was satisfactorily passed and we 

have used that WPS & PQR for the previous project 10 years ago and no 

issues found without PWHT.

 Now for the new project, we are going to use the same WPS and apply 

Preheat ( 204 to 250 Deg C ) as per the WPS for 10mm Shell Thk by 

multipass welding, refer to the below sketches.

<image.png>


<image.png>


So, i would like to confirm whether PWHT is mandatory as per UCS-56-4 ?

Can we avoid PWHT for this 10mm weld joint ?


Or Should we do buttering with ERNiCr-3 on P No.5A bevel and butt weld 

with same filler for this dissimilar joint to avoid PWHT after making new 

PQR with buttering?


Please confirm soon.


Thanks and Regards,

Saravanan Sornam,

ANSAN-Si,

S.Korea 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2Biby3LDhuASFD6Sx3wD6mhOVKRXA8dsJCQcfO-yNsjhQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

PARAI Reaction Channel

unread,
May 22, 2025, 10:36:40 PM5/22/25
to materials-welding@googlegroups com
Dear Sir, 

It is a condensate receiver tank and it is a design requirement from client side.

Regards, 
Saravanan. 
S.KOREA 

George Dilintas

unread,
May 23, 2025, 7:43:25 AM5/23/25
to material...@googlegroups.com
in case the nominal base metal thickness is less than 16 mm and the specified Cr% is less than 3 (you must check the base metal MTRs) and the max C% is 0,15 (check MTR) and you apply a min preheat of 150degC then you are allowed not to perform PWHT, as per Section I
Δρ. Γεώργιος Διλιντάς
Ηπείρου 5 , Μελίσσια - 15127
Αεροναυπηγος Μηχανικός - Μελος ΤΕΕ 55018
Τηλ +30 210 8100578, +30 6944 646 204

Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I,  Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis


PARAI Reaction Channel

unread,
May 25, 2025, 7:39:44 AM5/25/25
to materials-welding@googlegroups com
Dear Sir,

Thank you for your explanation. 

As the vessel design based on Sec VIII Div-1, and if our client  insists to do PWHT for that joint,
 Case 1) can we do a pqr by buttering with ERNiCr-3 on P No.5A plate and butt weld with same filler for this dissimilar joint to avoid pwht.

Because,  for P no.1 , the holding temperature is about 600 deg C and for P No.5A, the holding temperature is about 675 degrees C as per Sec VIII Div1,.

Case 2) Or , when we do pwht for this joint using ER80S-B2 filler,  can we use higher holding temperature of 675 degree C .

METALLURGICALLY, is it safe ?

Please confirm. 

Thanks and Regards, 
Saravanan Sornam, 
S.KOREA 




Reply all
Reply to author
Forward
0 new messages