SMAW +SAW

49 views
Skip to first unread message

Dharma dattu

unread,
Sep 5, 2019, 3:58:31 AM9/5/19
to Materials & Welding
Dear all,
Need to establish a WPS For a project with PWHT root(full penetration by SMAW)and Subsequent layers by (SAW).

My doubt is I have two seperate WPS for each procedure with PWHT separately.

Can I submit both WPS to client and use them as one procedure on job
1. Root- full penetration joint - SMAW
2. SUB sequent layers - SAW

NO Backgouging will be done.
Root and finish to be UT 100%.

REGARDS,

DATTU.

Dinesh Somwanshi

unread,
Sep 5, 2019, 8:20:42 AM9/5/19
to materials-welding
Yes.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1fe7d9fd-d244-4aea-ae2d-8bcda3ae1316%40googlegroups.com.

Vinay Thattey

unread,
Sep 12, 2019, 11:15:31 PM9/12/19
to material...@googlegroups.com

dharm...@gmail.com


Yes , I don't see any issue.

Dharma dattu

unread,
Sep 15, 2019, 11:14:30 AM9/15/19
to Materials & Welding
Can I submit two WPS and do weld on a single job with both ( root&hot pass by SMAW and Subsequent layers by SAW)
Reply all
Reply to author
Forward