REGARDING SAMPLE COPY OF CS PIPE TO SS PIPE WPS & PQR

65 views
Skip to first unread message

Kishor Swaminathan

unread,
Mar 18, 2021, 12:54:08 AM3/18/21
to Materials & Welding
Dear Experts ,

Anyone have WPS AND PQR  for CS Pipe to SS Pipe  

NOTE :  we want to weld:  SA240 GR.316L   to  API 5L GR.B PSL 
           Please check the attached drawing . we want to weld item no. 7 to item no.8


Thanks in advance 

KISHOR 
WELDING INSPECTOR 





7313-F-02029-001-01 (1).pdf

Xe đạp Ánh Dương

unread,
Mar 23, 2021, 4:26:16 AM3/23/21
to material...@googlegroups.com
If you plan to use the welding process GTAW, you can use the filler metal ER309L

Vào Th 5, 18 thg 3, 2021 vào lúc 11:54 Kishor Swaminathan <kish...@gmail.com> đã viết:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPd%2B2RTU%3DSUt8eJBTt7%2BZLsFAtia%3DYSRTDeBXu9-1sXQFYX2gw%40mail.gmail.com.

Kishor Swaminathan

unread,
Mar 24, 2021, 1:08:02 AM3/24/21
to Materials & Welding
good morning,
 yes  we will go to do the GTAW.

you have the WPS and  PQR 
please send me for sample 
i want to make new wps and pqr for this job.

Thanking you 

Kishor 