Welder Qualification (Pipeline Weldolet) Destructive Test Requirements

38 views
Skip to first unread message

Mahmood Alhinai

unread,
Aug 8, 2025, 11:49:52 PMAug 8
to material...@googlegroups.com
Dear Experts,

Please what are the destructive/mechanical tests required to qualify welder for branch weld (pipe 24 in 11.13 mm into weldolet 1 in sch 160) of pipeline as per API 1104 21st edition.

From which clause/table I can find the requirement?

Thanks,
Mahmood
 

Ch Bilal jovinda

unread,
Aug 9, 2025, 7:44:13 AMAug 9
to material...@googlegroups.com
Greetings,
Finde below detail for the referance.
1. Visually shall be accepted as per para 6.4.
2. For destructive tests, coupin for each welder shall be tested 4 no. Nick break and 4 no. Of side bend.
3. For non destructive test RT or PAUT as per client preffered method for production.

Best Regards,
Muhammad Bilal
Lead welding Engineer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANV5n6jRieMf15RpjozU67ggBprrpfvwN8VW9VGRy2XF2Dx2hg%40mail.gmail.com.

sridhar cn

unread,
Aug 9, 2025, 8:05:26 AMAug 9
to material...@googlegroups.com

Welder qualification for the specific branch weld requires welding a full-scale test coupon that replicates 

the branch weld dimensions, followed by destructive tests—primarily nick break, root bend, and face bend 

tests—prepared according to the specimen configurations in Figures 10 and 11, meeting requirements set 

forth in Clauses 5.7 and 6, and Tables 6 and 7 of API 1104, 21st edition.