BRIJESH KUMAR SINGH

unread,
Mar 21, 2013, 1:38:17 PM3/21/13
to material...@googlegroups.com

Dear seniors
I regularly fallow your all E-mails and query. Can any bady tel me how to prepare WPS & PQR.
I will really appropriate you if anyone help me for the above.

Thanks in advance

Subramaniyan Karunanidhi

unread,
Mar 22, 2013, 1:15:04 AM3/22/13
to material...@googlegroups.com
Hi,
Based on what code?
Regards,
Karun

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

BRIJESH KUMAR SINGH

unread,
Mar 22, 2013, 2:35:46 AM3/22/13
to material...@googlegroups.com

Sir
You can consider ASME.
Please tel me sir I want it for study purpose.
I am thankfull for  you response.

chandrakant mohikar

unread,
Mar 22, 2013, 2:32:17 AM3/22/13
to material...@googlegroups.com
You need to specify co. requirements for preparation.

you may refer

QW 100, 200 articles in ASME sec. IX

Chandrakant Mohikar (PMC)
(ex. Project-QA, PDO/ VELOSI Oman)


--

Nandesh Kumar

unread,
Mar 22, 2013, 5:38:15 AM3/22/13
to material...@googlegroups.com

Useful link :

http://www.wes.ir/files/2326318welding%20qualification.pdf

Also see attached

Also, you can search this forum. Many experts have given answers to your query clearly.


ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Fri, 22/3/13, BRIJESH KUMAR SINGH <brijeshkum...@gmail.com> wrote:

From: BRIJESH KUMAR SINGH <brijeshkum...@gmail.com>
Subject: Re: [MW:17192] How to make WPS & PQR
To: material...@googlegroups.com
Date: Friday, 22 March, 2013, 6:35 AM

Sir
You can consider ASME.
Please tel me sir I want it for study purpose.
I am thankfull for  you response.

On Mar 22, 2013 11:04 AM, "Subramaniyan Karunanidhi" <subra...@gmail.com> wrote:
Hi,
Based on what code?
Regards,
Karun
WPS-PQR Review Checklist 2007.pdf

Dinesh

unread,
Mar 22, 2013, 5:01:55 AM3/22/13
to material...@googlegroups.com

Dear sir,

 

Please read asme 9 & along with aws d1.1.First read aws d 1.1 so it will be easy to understand an some sort of information.

 

Regards

Dinesh

Chauhan Hemal

unread,
Mar 22, 2013, 7:32:13 AM3/22/13
to material...@googlegroups.com
Dear Mr. brijeshkumarji,


Please visit the following site for to making and review WPS/PQR....


Regards,
hemal chauhan,
Engineers india limited



From: Dinesh <som...@gmail.com>
To: material...@googlegroups.com
Sent: Friday, 22 March 2013 2:31 PM
Subject: RE: [MW:17195] How to make WPS & PQR

BRIJESH KUMAR SINGH

unread,
Mar 22, 2013, 9:06:33 AM3/22/13
to material...@googlegroups.com

Thank you sir
Your attachments are really help to me. Actually I was very confused that how to refer the codes because there is lots of articles and I was not sure to which I should take and which one not, but now I got the link to start my study.
Thank you very much sir