X-RAY Penetration Power

51 views
Skip to first unread message

pradip kumar Sil

unread,
Feb 9, 2026, 1:55:21 PMFeb 9
to materials-welding
Hi Everybody,

Can anyone tell me the required thickness for X-ray penetration of carbon steel and DSS materials as per EN/ISO/ASME codes? Please refer to the relevant code/ standard.  
Rgds

sridhar cn

unread,
Feb 12, 2026, 12:09:48 AMFeb 12
to material...@googlegroups.com

Penetration level: As per EN/ISO 17636-1

For CS:    ~30-200 mm (X-ray -1-4MeV Class A) ;   ~50-180 mm (Class B- Inspector training).

For DSS: Same above range as a base and to meet IQI.

 

Penetration level: As per ASME sec. V

 

For CS: No Specific limits. X-ray energy and technique to achieve required penetration and IQI sensitivity up to job thickness.

 

For DSS: Same above and to meet IQI for the thickness used.


Sridhar.

----------------------------------------------------------------------------------------------------------------------------------------------------------------------


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8nqrbvm2Kob_Z_Ybx0_V-ZL1c2ufk1VAQe6jU4QK5oDKA%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages