please advice welding of STRENX 700 with CS S275 and with it self 

attached MTC for your reference 

Regards,
H.A 
mtc.pdf

PGoswami

unread,
Nov 28, 2017, 10:39:12 AM11/28/17
to material...@googlegroups.com

Hi Hani,

 

Please see the attached datasheet for your reference. It’s the data sheet from the OEM. It’s not clear from your email, what’s the thickness to be welded. However welding with 100 Ksi (UTS) welding consumable would be challenging, cracking may occur for any unspecified reasons.

 

Also use the welding products of reputed vendors. Also ask for diffusible hydrogen test results and the CE values of the welds (equal or less than the BM),so as  to minimize cracking while welding. This is in addition to application  of preheat and control of interpass” temperature.

 

Note these steels are of very high tensile steel, hence application of  preheat and control of interpass temperature has to selectively decided , upon consultation with the OEM and consumable vendors.

 

Thanks,

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@quickclic.net,pradip....@gmail.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


Virus-free. www.avg.com
Welding-of-Strenx-Advanced-High-Strength-Steels.pdf

Hani Al Masry

unread,
Nov 29, 2017, 5:15:11 AM11/29/17
to material...@googlegroups.com
Dear P.Goswami

thanks 
as per MTC thick. is 20mm 
SSAB recommended to use 7018 OR 9016 without any application of  preheat and control of inter pass temperature

Regards,
H.A 

On Tue, Nov 28, 2017 at 7:38 PM, PGoswami <pgos...@quickclic.net> wrote:

Hi Hani,

 

Please see the attached datasheet for your reference. It’s the data sheet from the OEM. It’s not clear from your email, what’s the thickness to be welded. However welding with 100 Ksi (UTS) welding consumable would be challenging, cracking may occur for any unspecified reasons.

 

Also use the welding products of reputed vendors. Also ask for diffusible hydrogen test results and the CE values of the welds (equal or less than the BM),so as  to minimize cracking while welding. This is in addition to application  of preheat and control of interpass” temperature.

 

Note these steels are of very high tensile steel, hence application of  preheat and control of interpass temperature has to selectively decided , upon consultation with the OEM and consumable vendors.

 

Thanks,

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@quickclic.net,pradip....@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hani Al Masry
Sent: November 28, 2017 5:32 AM
To: materials-welding@googlegroups.com
Subject: [MW:27062] Welding of PLATES STRENX 700

 

Dear All

 

please advice welding of STRENX 700 with CS S275 and with it self 

 

attached MTC for your reference 

 

Regards,

H.A 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages