Dear Sirs,

One of our client asked us to test FN using Ferritescope for the weld samples of 10T and 6T Singe V Butt Joint, made using A240 -.316 and A 516-70 , welded with GTAW ER309.

The values recorded as 4.7, 4.3, 4.7 in 10T and  2.1, 2.2, 1.9 in 6T.

So, why this much difference by using same GTAW AWS Class ER309 rod, but welded in two different "T" samples with bit change in welding parameters.

What is the acceptance criteria for FN of 309 welding? 

As per ASME Sec II C, SFA 5.9 for 309 type, it is given as 12 FN, if I am right.
So, can I use this as a reference for acceptance criteria

Please advice.

Regards,
Saravanan,
Pyeongtaek,
Korea
 

Prakash Hegde

unread,
Sep 9, 2019, 3:38:51 AM9/9/19
to material...@googlegroups.com
Hi
It is surprising that you get Fn so low for 309 weld Generaly you get 12 to 15 for 309 grade weld
Regards
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkLinuq22CP8wpf9SCub9iApmCKwKrfLaEXpETYM%2BkqUQw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages