G.K.PILLAI

unread,
May 31, 2019, 3:58:33 AM5/31/19
to material...@googlegroups.com
Hi  Gents, 

I have one doubt that we qualified two wps for branch connection as per bsen 15614-1 with branch angle 35degree , main pipe die 800mm branch pipe dia 400mm root gap 2- 5 mm without backing strip and another one wps  is same as above only different that rootgap  8-20 mm (widegap) with backstrip.test results was acceptable. in this both wps can i have to use the single joint .it means  the same degree of the branch joint  half of the joint where ever rootgap 2-5 mm  with out backstrip and another half of the joint wherever root gap 8-20 mm  with back strip based on above wps.please confirm.



Thanks&Regards,

G.K.PILLAI.

MOBILE

+919500755882   (INDIA)

pradip kumar Sil

unread,
May 31, 2019, 9:02:51 AM5/31/19
to materials-welding
Backstrip & root gap is not essential variable but particular case you should change variable data

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACmDAmVOTLA_NMGdjVx2C6sZ46ysefu%2BKpSLO53rRBujd7BaRQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Vinay Thattey

unread,
Jun 3, 2019, 10:18:39 AM6/3/19
to material...@googlegroups.com
Can you add information about thickness or schedule.

--