EN5817 / ISO 17635

321 views
Skip to first unread message

Shashank Vagal

unread,
Oct 13, 2010, 7:27:57 AM10/13/10
to material...@googlegroups.com
Hi all,
One query seen on some other site. I feel it could be of interest to our members as well.

When working to the standard EN5817 - Quality levels for imperfections, it states ISO 17635 is to be used for a correlation between the quality level and acceptance level for different NDT methods. (EN5817 is directly applicable to VT only as stated in its introduction)

 ISO 17635 - General rules for metallic materials (2010 version) states UT is to be performed in accordance with ISO17640 (instead of the usual EN1714) and the acceptance level to be used is ISO11666 (instead of the usual EN1712).

I am not familiar with these new ISO standards, and when I went to purchase them from the British Standards site I couldn't find them? On the French equivalent site (AFNOR) it states that these specifications are still in draught form??

Does that mean we should still be using the EN standards, which would then go against the requirements of ISO 17640. Or are these ISO standards word for word the same as the EN standards?

Has anybody come across this problem yet??

Any suggestions?
Best regards,
Shashank Vagal

Karthik

unread,
Oct 13, 2010, 10:16:27 PM10/13/10
to material...@googlegroups.com
Hi,
Please find herewith the attached file of Overview of European (INternational) standards for fusion welding with ISO reference.
Please note that ISO reference in most cases are identical with or its based on EN standards.
 
If you want to purchase ISO standards please go to www.iso.org
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 10/13/10, Shashank Vagal <nach...@yahoo.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Overview_fusion_welding_standards.pdf
Reply all
Reply to author
Forward
0 new messages