API 1104 WELDER QUALIFICATION

274 views
Skip to first unread message

thulaib arakkal

unread,
Apr 28, 2024, 1:23:29 PM4/28/24
to material...@googlegroups.com
Hi All,

If I qualify a pipe welder in 6G position as per API 1104, is he qualified to weld in 5G position. Please note as per API 1104 not ASME.

Regards, 

Thulaib 

saleem manhappulath

unread,
Apr 28, 2024, 1:35:25 PM4/28/24
to material...@googlegroups.com
Yes, it’s qualified in 5g also


Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JOm6hejgTvoEJj8ELnjkKVyRSUqtM%2BRmMRZKe2RUyDb%3DA%40mail.gmail.com.

Unnikrishnan K.S

unread,
Apr 28, 2024, 2:33:05 PM4/28/24
to material...@googlegroups.com
Yes he qualifies all positions 

Thanks and Regards,

K.S.Unnikrishnan
Kollara

On 28-Apr-2024, at 9:23 PM, thulaib arakkal <thulaib...@gmail.com> wrote:


--

Bechir TLILI

unread,
Apr 28, 2024, 2:33:08 PM4/28/24
to material...@googlegroups.com
Yes, 

--

Amol Betkar

unread,
Apr 29, 2024, 6:01:43 AM4/29/24
to material...@googlegroups.com
Dear,

Yes, according to API 1104, if a pipe welder is qualified in the 6G position, they are generally considered qualified to weld in the 5G position as well. API 1104 typically covers welding standards and procedures for pipeline welding, and it doesn't specifically differentiate between 5G and 6G positions in terms of qualification requirements for welders. Therefore, a qualification in the more challenging 6G position typically implies proficiency in welding positions of equal or lesser difficulty, such as the 5G position. However, it's always essential to review the specific requirements of API 1104 and any relevant project specifications to ensure compliance.

Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)

james gerald

unread,
Apr 29, 2024, 10:35:58 AM4/29/24
to material...@googlegroups.com
Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



--

Muhammad Asif

unread,
May 4, 2024, 2:39:51 AM5/4/24
to material...@googlegroups.com
Dear Thulaib,

A welder qualified in 6G position is qualified for all positions. 


--