Dear Sir,,


I have one PQR with 3 mm GTAW weld deposit and 6.5 mm SMAW deposit. Base metal thickness is 9.5 mm and impact is not required.

Please correct me if any of the following is NOT correct as per Sec IX

1) Combined Process (GTAW + SMAW) up to a thickness of 1.5 to 19 MM (2T)

2( Single process wps of SMAW with weld metal thicjness 13 MM and qualified base metal thickness is 1.5 mm to 13 mm

3)  Single process WPS of GTAW  with weld metal thickness of 6 MM and Qualified base metal thickness is 1.5 to  6 mm




Please help!!

Riaz 

james gerald

unread,
Aug 6, 2015, 2:39:53 AM8/6/15
to material...@googlegroups.com
irrespective of single process GTAW / SMAW used the BASE METAL thickness range qualified is  1.5 - 19mm

others acceptable.

Thanks & Regards
J.Gerald Jayakumar
0091-9344954677


From: "Ri@z" <riaz.r...@gmail.com>
To: Materials & Welding <material...@googlegroups.com>
Sent: Thursday, August 6, 2015 11:56 AM
Subject: [MW:23271] Multiple WPS from single PQR

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b3a24345-befb-4d5c-b65a-9cfc47a53889%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Bijay

unread,
Aug 6, 2015, 2:55:54 AM8/6/15
to materials-welding@googlegroups com
But for SMAW single process you have to give Metal baking as the GTAW weld Metal act as metal baking.

Sent from Yahoo Mail on Android


From:"Ri@z" <riaz.r...@gmail.com>
Date:Thu, 6 Aug, 2015 at 11:58 am

Subject:[MW:23271] Multiple WPS from single PQR

george....@gr.bureauveritas.com

unread,
Aug 6, 2015, 4:32:14 AM8/6/15
to 'Bijay' via Materials & Welding
Backing is a welders qualification essential variable. For PQR it is a nonessential one.
The Base metal qualification range is the same for the 3 cases

Sent from my BlackBerry 10 smartphone.
From: 'Bijay' via Materials & Welding
Sent: Πέμπτη, 6 Αυγούστου 2015 - 09:55
To: materials-welding@googlegroups com
Subject: Re: [MW:23273] Multiple WPS from single PQR


For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Don Under Survilliance

unread,
Aug 6, 2015, 6:23:37 AM8/6/15
to material...@googlegroups.com, riaz.r...@gmail.com
Backing is a non-essential variable for PQR.

for your information . to the best of my knowledge.

Regards,

Ajay Kadyan

EIL

On Thu, Aug 6, 2015 at 3:09 PM, Don Under Survilliance <dons...@gmail.com> wrote:
Dear Riaz

Ur understanding is absolutely correct as per QW 451.1 of sec IX. However, WPS for SMAW will be with Backing.




Regards,

Ajay Kadyan
EIL

Ri@z

unread,
Aug 6, 2015, 6:24:24 AM8/6/15
to Materials & Welding

Thank You For reply


My humble doubt is, 1 ) weld metal deposition is restricted to be max 6 mm for gtaw, and 13 mm for SMAW, what is the advantage of having 19 mm as  Qualified base metal thickness. For separate process there is no advantage of Base metal Qualified as per QW-451 ie 1.5 to 2T

AM I RIGHT ???

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1438843327.97025.YahooMailAndroidMobile%40web181301.mail.ne1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Don Under Survilliance

unread,
Aug 6, 2015, 6:50:12 AM8/6/15
to material...@googlegroups.com, riaz.r...@gmail.com
Dear Riaz,

Advantage is to reduce the no of WPS. A single PQR (Combined process) can be used to prepare three different WPS or even more within the range qualified for weld deposit and base metals thickness.

Further, in WPS, we also mentioned the range qualified for individual processes.

This is best of my knowledge. if I am wrong, correct me,

Regards,

Ajay Kadyan
Engineers India Limited.



To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b3a24345-befb-4d5c-b65a-9cfc47a53889%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1438843327.97025.YahooMailAndroidMobile%40web181301.mail.ne1.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

george....@gr.bureauveritas.com

unread,
Aug 6, 2015, 8:45:39 AM8/6/15
to Ri@z
Many advantages like:
1. Partial penetration welds
2. Combination with other processes 
3. Welding of small bore piping with GTAW


Sent from my BlackBerry 10 smartphone.
From: Ri@z
Sent: Πέμπτη, 6 Αυγούστου 2015 - 13:24
To: Materials & Welding
Subject: Re: [MW:23276] Multiple WPS from single PQR


For more options, visit https://groups.google.com/d/optout.

james gerald

unread,
Aug 7, 2015, 10:33:37 AM8/7/15
to material...@googlegroups.com
Inaddition to what George has highlighted

1. For a dissimilar thickness weld between Base Material 6mm thick to 19 mm thick example like a shell to dished End and a skirt to a shell.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677


From: "george....@gr.bureauveritas.com" <george....@gr.bureauveritas.com>
To: "Ri@z" <material...@googlegroups.com>
Sent: Thursday, August 6, 2015 6:15 PM
Subject: Re: [MW:23280] Multiple WPS from single PQR

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.

For more options, visit https://groups.google.com/d/ optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer. bureauveritas.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cba069da-c9e1-4902-9e1d-bbefd56859c0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
Reply all
Reply to author
Forward
0 new messages