REQUIREMENT OF NACE MR0175 FOR SA182 F316L TO SA213-TP316L WELDING.

160 views
Skip to first unread message

sujit kumar

unread,
Feb 3, 2023, 3:45:34 AM2/3/23
to Materials & Welding
Dear experts,


What is the requirement of NACE MR0175 to weld  SA182 F316L TO SA213 TP316L 
if there any Hardness require for that....???

is there is any special requirement for WPS PQR...???

NOTE:-SA182 F316L TO SA213 TP316L this material is also NACE Material.


Best regards
sujit.

Prasad rao

unread,
Feb 5, 2023, 10:01:44 PM2/5/23
to material...@googlegroups.com
Dear Sujith ,

There are no specific requirements mentioned about hardness values for SS/DSS/DSS/CRA , If you can refer to NACE MR0103 states the same for you please refer to the below may be useful.
image.png

With Regards,
Prasad rao.



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/528c875c-6491-4e44-9656-3bc30beb340bn%40googlegroups.com.

P Goswami

unread,
Feb 6, 2023, 11:14:53 AM2/6/23
to material...@googlegroups.com

Hi Sujit,

 

MR-0175 is a history, it’s replaced by ISO-15156. See the snapshot of the appropriate sections of this specification for your reference. Your query is not very specific. Is the intended design/operating service being Sour Environment as classified by NACE?

If that’s the requirement then it’s advisable to perform hardness survey on the weld cross section.

You may see the appropriate extracts from ISO-15156-3 , for your reference.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Cell/Whasapp:1-905-9793232

 

 

 

From: Prasad rao <prasa...@gmail.com>
Sent: February 3, 2023 10:56 PM
To: material...@googlegroups.com
Subject: Re: [MW:33990] REQUIREMENT OF NACE MR0175 FOR SA182 F316L TO SA213-TP316L WELDING.

 

Dear Sujith ,

 

There are no specific requirements mentioned about hardness values for SS/DSS/DSS/CRA , If you can refer to NACE MR0103 states the same for you please refer to the below may be useful.

 

With Regards,

Prasad rao.

 

 

 

On Fri, Feb 3, 2023 at 12:45 PM sujit kumar <sujitku...@gmail.com> wrote:

Dear experts,

 

 

What is the requirement of NACE MR0175 to weld  SA182 F316L TO SA213 TP316L 

if there any Hardness require for that....???

 

is there is any special requirement for WPS PQR...???

 

NOTE:-SA182 F316L TO SA213 TP316L this material is also NACE Material.

 

 

Best regards

sujit.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/528c875c-6491-4e44-9656-3bc30beb340bn%40googlegroups.com.


Virus-free.www.avg.com
image007.png
image008.png
image014.png
image015.png
image016.png
image017.png

james gerald

unread,
Feb 6, 2023, 9:58:11 PM2/6/23
to material...@googlegroups.com
Mr. Goswani was up to the point on the Hardness requirement for parent metal & PQR for CRA.

Just to Add, ISO 15156 -1/2/3 is applicable only for upstream Oil facilities for the below

Inline image
Requirements for carbon and LAS steel sour service requirements are quite simple and governed below.

Inline image
Whereas the Requirement of sour service for CRA is Quite complex and governed by many factors as below.

Inline image
Hence for the applicable Requirements, the proper Table for CRA shall be selected and made Applicable.

Inline image

Thanks & Regards

J.Gerald Jayakumar




Reply all
Reply to author
Forward
0 new messages