Flange Connection

22 views
Skip to first unread message

Madhan S

unread,
Mar 17, 2017, 11:53:58 PM3/17/17
to Materials & Welding
Dear All,

We need to connect a Flanged Gate valve (RF) with Flange Adapter (FF). We are going to use full-faced EPDM gasket.

My questions are,
1. Will it be a leak tight joint?
2. Is it accepted as per code? (If Yes, Please give me reference standards)


Thanks & Regards,
Madhan. S

Hemant W Joshi

unread,
Mar 20, 2017, 12:34:02 AM3/20/17
to material...@googlegroups.com

Why is a full faced gasket required when a flat ring would be sufficient ?

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/238a0a02-7080-4ab5-9199-95b3f0a27ba6%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------

Reply all
Reply to author
Forward
0 new messages