I am involved in maintenance of Boiler pressure parts, kindly help me
by providing some sort of ready reckoner for selection of filler rods
for welding similar & dissimilar metals. Eg. SA 210 GrA1 to SA 210 GR
A1, SA 213 T11 to SA 213 T22, SA213 T22 to SA 335 P22.

With Regards,

Chella

Bathula Raghuram (Mumbai - PIPING)

unread,
Jul 6, 2010, 12:43:47 AM7/6/10
to material...@googlegroups.com
You may refer the attachment for dissimilar combination, and you can get a copy of complete welding manual from http://www.boehler-welding.com/, due to space constraint I am not posting it in the group

Dear Members,

With Regards,

Chella


Filtered by Hosted Filtering

Pages from Welding_Guide_2008_EN_verlinkt.pdf

Nandesh Kumar

unread,
Jul 6, 2010, 8:48:00 AM7/6/10
to material...@googlegroups.com
Chella,
 
Attached document may be helpful to you.
 
Regards,
Nandesh Kumar A

--- On Tue, 6/7/10, Chella <m.chel...@gmail.com> wrote:

From: Chella <m.chel...@gmail.com>
Subject: [MW:5868] Select Filler Rods For Welding Similar & Dissimilar Metals
To: "Materials & Welding" <material...@googlegroups.com>
Date: Tuesday, 6 July, 2010, 4:31 AM

Dear Members,

I am involved in maintenance of Boiler pressure parts, kindly help me
by providing some sort of ready reckoner for selection of filler rods
for welding similar & dissimilar metals. Eg. SA 210 GrA1 to SA 210 GR
A1, SA 213 T11 to SA 213 T22, SA213 T22 to SA 335 P22.

With Regards,

Chella

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Electrode_selection.pdf
Reply all
Reply to author
Forward
0 new messages