Dear Sir,


I am confusing for EGW welder operator thickness qualified because we conduct test for welder operator on thickness 16.0 mm plates which are single pass only.  As per ASME-IX  QW-403.9 For singlepass or multi pass welding in which any pass is greater than 1/2 in. (13 mm) thick, an increase in base metal thickness beyond 1.1 times that of the qualification test coupon. Can anyone clarify me maximum thickness qualified welder operator.

 

Regards

Anamul

QA/QC Engineer

george....@gr.bureauveritas.com

unread,
Jan 29, 2016, 5:08:10 AM1/29/16
to material...@googlegroups.com

It is restricted by the WPS only

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS A.E  - PIRAEUS  GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

anam...@gmail.com

unread,
Feb 2, 2016, 8:24:47 AM2/2/16
to Materials & Welding
Dear Sir,
Thank you for your valuable comments.