Hi,
Lap joint is welded by fillet weld and if you have 1 g qualified wps / PQR
then you can very well use the same for Lap joint.
On Sat, 29 Oct 2011 20:20:59 +0530 wrote
welding+u...@googlegroups.com
For more options, visit this group's bolg at
http://materials-
welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
Dear Sir,
Thanking You,
Honesty is the best Policy
With Warm Regards,
Muthu Barathi P