Dear All

According to ASME sec IX, for GTAW, FCAW and GMAW in supplementary essential variables (QW 410.9) , a multi pass per side fillet/butt weld procedure cannot be used to weld single pass per side. (say single pass per side fillet weld.)
I am curious to know the technical reason behind the same. In my opinion, fill pass parameters of a butt weld procedure can be used for welding single pass fillet welds. Please advice if this is incorrect and kindly provide technical/ metallurgical reasoning for the same.

Thanks & best regards

Kathalingam Babu

unread,
Apr 25, 2011, 11:40:19 PM4/25/11
to material...@googlegroups.com
Hi
 
It is because of the reason that, in multipass weld will be tempered and refined by subsequent passes but in case of Single pass will not be.
 
That is the reason , multipass to single pass is considered as SEV, but not vice versa.
 
Thanks & Regards,
 
K. Babu

----- Original Message -----
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Reply all
Reply to author
Forward
0 new messages