4130 P no.

39 views
Skip to first unread message

Vikas Bhandari

unread,
Jun 2, 2015, 3:59:48 AM6/2/15
to material...@googlegroups.com
Dear all

Does 4130 has a designated P no. is ASME IX?

Table 333.1.1 (Post weld heat treatment) of ASME B31.3 gives maximum heat treatment temperature restrictions. 

I was wondering if it is an unassigned material, these restrictions will not apply?


Any thoughts..

Prakash Gotimukul

unread,
Jun 2, 2015, 4:56:15 AM6/2/15
to materials-welding
Section 333.1.1 shall prevail

Rgds
G.Prakash
AIS, AIA LLC TX, USA

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACpSjO%3DL8zutjgiGOT8uJ7-Fh1t3TxevQC3MnuBkNVBCWbnemw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages