Inter Granular Corrosion in Carbon Steels

91 views
Skip to first unread message

Zacharias Rohith Joseph

unread,
Feb 16, 2021, 1:36:41 AM2/16/21
to Materials & Welding
Hello everyone., 

Can someone pls explain the possibility of IGC in carbon steels. I was of the opinion that the same is more predominant  in exotic steels  like nickel or chrome based. 

what can be possibility of IGC occurring in carbon steels? 

Vishwas Keskar

unread,
Feb 16, 2021, 1:51:26 AM2/16/21
to material...@googlegroups.com
Carbon steel is not used when corrosion is envisaged in equipment service .

IGC is observed in TYP 304 materials  



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/13fa8001-fd5e-42ea-a7a0-f4a47579db8an%40googlegroups.com.

Vinay Thattey

unread,
Feb 17, 2021, 11:44:25 PM2/17/21
to material...@googlegroups.com
Dear Friend ,  The IGSCC or intergranular stress  corrosion is attributed to precipitation of chromium carbide at grain boundary. Also a favourable environment and a temperature range for sufficient time period boosts IGSCC . 