Dear All,
 
let me know how to select the IQI wire of carbon steel 6inch sch 80 reference code is B31.3 material as P1 please reply me as soon as possible.
 
Thanks & Regards
venkat (QC)

Sakib

unread,
Aug 2, 2010, 2:12:28 AM8/2/10
to material...@googlegroups.com
See the attachement it will be helpful to you
--
with Regards


SAQIB JALAL
Inspection Engineer
PakArab Fertilizer Limited
Khanewal Road , Multan
office number +92-61-9061 EXT 3110
mobile number +92-321-4043556
IQI TABLE.pdf

Nandesh Kumar

unread,
Aug 2, 2010, 3:25:54 AM8/2/10
to material...@googlegroups.com
Venkat,
 
Which IQI? ASTM, DIN(ISO), FE EN? all differes and depends upon thickness of the object being radiographed...Diameter is not  a concern.
 
regards,
Nandeesh

--- On Mon, 2/8/10, venkat ramana <venkatgp...@gmail.com> wrote:
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Tran Van Vuong

unread,
Aug 2, 2010, 3:54:08 AM8/2/10
to material...@googlegroups.com

Dear Venkat

 

Applicable test standards: ASME Sect. V Art.2 for procedure, Pipe 6” SCH80, norm. Thk 11.0. Exp. Technical: DWSI, IQI on film side, essential wire number 6 (dia. 0.25) So you can select ASTM 1A 6 or ASTM 1B 11.

 

 

Best regards

 

TRAN VAN VUONG

Email: vuo...@phateco.com


image001.gif
image002.gif

tong tong

unread,
Aug 2, 2010, 4:41:02 AM8/2/10
to material...@googlegroups.com

Don't forget to add reinformence cap height in order to get the material thickness range
Regards 
image002.gif
image001.gif

Tran Van Vuong

unread,
Aug 2, 2010, 5:03:45 AM8/2/10
to material...@googlegroups.com

Dear Venkat

Thickness of weld does not include any reinforcement as ASME specified.

 

Best regards

 

TRAN VAN VUONG

Email: vuo...@phateco.com

image001.gif
image002.gif

george....@gr.bureauveritas.com

unread,
Aug 2, 2010, 9:33:54 AM8/2/10
to materials-welding

Sorry but you should refer to T276.2(a) of section V


image001.gif
image002.gif

Leo Sudarmadji

unread,
Aug 2, 2010, 1:24:43 PM8/2/10
to material...@googlegroups.com
This for sample, 6" sch 80 is 0.432 in (10.973 mm) if Low pressure it would be 13.973mm thickness + reinforcement included, use ASTM 1B or 10 FE EN
 
Make sure ASTM or EN or what kind IQI mentioned in RT procedure.
 
 
Leo Sudarmadji
RT Supv.
image001.gif
image002.gif

tong tong

unread,
Aug 2, 2010, 7:03:48 PM8/2/10
to material...@googlegroups.com
Welds With Reinforcements. The thickness on which
the IQI is based is the nominal single-wall thickness plus
the estimated weld reinforcement not to exceed the maximum
permitted by the referencing Code Section. Backing
rings or strips shall not be considered as part of the thickness
in IQI selection. The actual measurement of the weld
reinforcement is not required.


On Mon, Aug 2, 2010 at 9:33 PM, <george....@gr.bureauveritas.com> wrote:

Sorry but you should refer to T276.2(a) of section V


image001.gif
image002.gif

DOKKU AJAY

unread,
Aug 3, 2010, 4:34:46 AM8/3/10
to material...@googlegroups.com
Please refer T-276.2 (a) & (b) for queries related to  consideration of weld reinforcement.


From: tong tong <ton...@gmail.com>
To: material...@googlegroups.com
Sent: Tue, August 3, 2010 2:03:48 AM
Subject: Re: [MW:6267] How to select the IQI wire
image001.gif
image002.gif

Raheel Arif

unread,
Aug 31, 2013, 2:55:51 AM8/31/13
to material...@googlegroups.com
Dear All,

Let me know what is the difference between ASTM, FE EN & DIN wire. What material is suitable for which wire?

Regards,
Raheel Arif

Dinesh Somwanshi

unread,
Aug 31, 2013, 4:56:45 AM8/31/13
to material...@googlegroups.com
the selection of IQI wirE type or hole type is thickness based on the sensitivity reqd.asme 5 IQI SELECTION AS WELL AS APPLICABLE CODE AWS D 1.1,ANSI B 31.3.,ANSI B 31.1 ALSO GIVES THE REQD FOR IQI SELECTION.

REGARDS

DINESH


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/

 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

CHINTUKUMAR GANDHI

unread,
Sep 1, 2013, 6:32:15 AM9/1/13
to material...@googlegroups.com
Dear Mr. Raheel/ Venkat,

If no project spec. is applicable, selection of IQI shall be as per Table T-276 of Article 2 of ASME Sec. V. For material selection group please refer SE-747 of ASME Sec. V.

Thanks & regards,


C. R. GANDHI          


From: Raheel Arif <rahe...@gmail.com>
To: material...@googlegroups.com
Sent: Saturday, August 31, 2013 12:25 PM
Subject: [MW:18547] Re: How to select the IQI wire

--
Reply all
Reply to author
Forward
0 new messages