welding of Nelson studs to HP profiles

25 views
Skip to first unread message

Emad Elgin

unread,
Aug 13, 2016, 1:01:00 AM8/13/16
to material...@googlegroups.com
We have welding of Nelson studs to HP profiles

do we need to have WPS/PQR? 

Please advice

Regards,
H.A

cheng chen

unread,
Sep 1, 2016, 3:15:36 AM9/1/16
to Materials & Welding
  
   AWS D1.1-2015 chapters 7.
hanyon於 2016年8月13日星期六 UTC+8下午1時01分00秒寫道:
擷取SW.PNG