Threading inspection according to API,VAM,Tenaris etc ?

414 views
Skip to first unread message

mpk mpk

unread,
Jan 2, 2012, 10:13:38 PM1/2/12
to materials-welding
Dear Experts,


 Can anybody share information relating threading inspection according to API,VAM,Tenaris etc., ?

Thank you
MPK

murali krishnan

unread,
Jan 16, 2012, 4:51:58 AM1/16/12
to material...@googlegroups.com
Dear Mr.MPK,
 
Refer API 5B - Specification for Threading, Gauging, and Thread Inspection of Casing, Tubing, and Line Pipe Threads (US Customary Units) (Includes March 2004 Addendum)
 
Click on the below link to download the specification.
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
G.Murali krishnan

Reply all
Reply to author
Forward
0 new messages