HDPE Pipe INSTALLAITION ITP&WPS

1,789 views
Skip to first unread message

Ramesh

unread,
Apr 1, 2013, 11:38:12 PM4/1/13
to material...@googlegroups.com
Dear all,
Any one can send HDPE PIPE under ground piping ITP &WPS FORMAT
 Thanks
RAMESH 
 
 
 

mohdfirdaus...@gmail.com

unread,
Apr 1, 2013, 11:57:06 PM4/1/13
to material...@googlegroups.com, material...@googlegroups.com
WPS?. I think there is no need for WPS. 2 type of fusion, electro fusion & butt fusion. It better you google it first before asking. Trust me, you'll find the solution when you google it. I found there too. 

Mohd Firdaus Abd Rahim
QA/QC

Sent from my iPhone
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

manpreet

unread,
Apr 2, 2013, 8:52:56 PM4/2/13
to material...@googlegroups.com
Firdaus,

Refrain from commenting if you don't have the correct information, yes there are WPS for HDPE pipe.

Ramesh,

Inbox me a request and I will send you a copy.

Cheers

Get your own FREE website and domain with business email solutions, click here

mohd firdaus abd rahim

unread,
Apr 3, 2013, 3:03:03 AM4/3/13
to material...@googlegroups.com
Please find the attachment. This I got from Mr. Google.

On Wed, Apr 3, 2013 at 2:53 PM, <mohdfirdaus...@gmail.com> wrote:
Ramesh,

Actually I have the complete procedure for HDPE Pipe underground work. From the details procedure we can create the ITP. HDPE Pipe usually use fusion method either butt fusion or electro fusion. Can you give me jointing method for your work?. Details material use, PN number, size & thickness, product name. I'll try my best to help you.


Mohd Firdaus Abd Rahim
QA/QC

Sent from my iPhone



--
Best Regard,

Mohd Firdaus Bin Abd Rahim
            seemys...@yahoo.com
7100-xxxx-HDPE.pdf
DoandDontsforPolyethyleneJointing.pdf

mohdfirdaus...@gmail.com

unread,
Apr 3, 2013, 2:53:45 AM4/3/13
to material...@googlegroups.com, material...@googlegroups.com
Ramesh,

Actually I have the complete procedure for HDPE Pipe underground work. From the details procedure we can create the ITP. HDPE Pipe usually use fusion method either butt fusion or electro fusion. Can you give me jointing method for your work?. Details material use, PN number, size & thickness, product name. I'll try my best to help you.

Mohd Firdaus Abd Rahim
QA/QC

Sent from my iPhone
On 03/04/2013, at 8:52 PG, "manpreet " <manpre...@rediffmail.com> wrote:

Ramesh

unread,
Apr 3, 2013, 3:56:01 AM4/3/13
to material...@googlegroups.com
Dear sir,
Kindly find the below details for HDPE PIPE for Under ground work  Fire fight/ form
PN 25
SIZE 3" TO 18"
7.4 PE 100/PN25
fusion method butt fusion
for procedure and ITP &WPS Can send me...
Balakrishnan Ramesh
QA/QCWelding Engineer
 
P.O. Box 10869, Dubai, U.A.E 

John Henning

unread,
Apr 3, 2013, 9:46:45 AM4/3/13
to material...@googlegroups.com

FYI:  The next edition of ASME Section IX will include fusion of HDPE. 

 

John A. Henning

Welding & Materials


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

hashi...@gmail.com

unread,
Jun 16, 2019, 4:31:03 AM6/16/19
to Materials & Welding
Please forward me a HDPE Fusion Welding procedure

GENE MATSKO

unread,
Jun 18, 2019, 5:59:14 AM6/18/19
to material...@googlegroups.com
Go to Google and search for HDPE procedure. McElroy and Dura Line also have good information

Gene Matsko


On Sunday, June 16, 2019, 03:31:02 AM CDT, <hashi...@gmail.com> wrote:


Please forward me a HDPE Fusion Welding procedure

---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages