Welding repair procedure required. (ASME or AWS)

826 views
Skip to first unread message

Mohammed Ghani

unread,
Jan 5, 2016, 2:19:32 AM1/5/16
to material...@googlegroups.com
Dear Expert,

I need welding repair procedure for structures, were can i find standard repair procedure (ASME or AWS).

Kindly guide for the welding repair procedure for structural welding


Regards

--
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.
Mechanical Inspector,
ü Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

Sadique Sheikh

unread,
Jan 5, 2016, 2:46:43 AM1/5/16
to material...@googlegroups.com
Dear Ghani,

Please refer in AWS D 1.1 clause 5.15.1.2 for repair procedure

Thanks & Regards,

Mohd. Sadique Sheikh


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG7AWVibiLirL%2BfTdu2K1JbMjYfFy-jxdCOzneGmC0JpK%2BbBTg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

JERRY TUAN

unread,
Jan 15, 2016, 8:56:09 PM1/15/16
to Materials & Welding
Yeah . I my idea , cause the spec aws d1.1 did not show how to qualify a welding repair procedure , so I think we can use the wps that we are already running on for build new structure to use for repair procedure .
In detail: if u have wps SMAW process for fabricate new structure, u can use that wps for repair also .

Kindly share my idea , if all experts here have any confirm or right info , please show with us

Thanks all experts
Tuan QC inspector

Dineesh

unread,
Mar 27, 2017, 8:31:30 AM3/27/17
to Materials & Welding
Dear Ghani,
Repair. In the repair and determination of
limits of mill induced discontinuities visually observed
on cut surfaces, the amount of metal removed shall be
the minimum necessary to remove the discontinuity or to
determine that the limits of Table 5.4 are not exceeded.
However, if weld repair is required, sufficient base metal
shall be removed to provide access for welding. Cut surfaces
may exist at any angle with respect to the rolling
direction. All welded repairs of discontinuities shall be
made by:
(1) Suitably preparing the repair area
(2) Welding with an approved low-hydrogen process
and observing the applicable provisions of this code
(3) Grinding the completed weld smooth and flush
(see 5.24.4.1) with the adjacent surface to produce a
workmanlike finish.
Note: The requirements of 5.15.1.2 may not be adequate
in cases of tensile load applied through the thickness of
the material.

Thanks with Regards'
Atif Aslam (Din).