Interpass temp

252 views
Skip to first unread message

saleem manhappulath

unread,
Jul 14, 2024, 8:11:35 AM7/14/24
to material...@googlegroups.com
Dear All

    we are used material ASTM A572 Gr 50 and Electrode E11018m for PQR ,
Maximum Interpass how much we can mention in the WPS

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

R S

unread,
Jul 14, 2024, 11:36:39 AM7/14/24
to material...@googlegroups.com
Dear, 

this is specific electrode, E11018M, the manufacturer's recommendations may vary. Typically, the manufacturer's instructions should be followed.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omv0KmS7%2B%2B-369L1K%2BOp5OHXZuj-RkTJ_n0_B2GmosZNLw%40mail.gmail.com.

krishnan T

unread,
Jul 14, 2024, 2:00:54 PM7/14/24
to material...@googlegroups.com
Reply i got From AI is below 

The interpass temperature when welding ASTM A572 Gr 50 with electrode E11018M (ENiCrMo-3) depends on the specific welding procedure and project requirements. However, here are some general guidelines:

- The interpass temperature for welding ASTM A572 Gr 50 typically ranges from 150°F to 300°F (65°C to 150°C).
- For electrode E11018M, the recommended interpass temperature is usually between 200°F to 250°F (90°C to 120°C).
- It's essential to consult the welding procedure specification (WPS) and the electrode manufacturer's recommendations for specific interpass temperature limits.
- Maintaining the appropriate interpass temperature helps prevent weld defects, ensures proper weld penetration, and achieves the desired mechanical properties.

Remember to always consult the relevant welding codes, standards, and project specifications for the specific interpass temperature requirements.

Prathab P

unread,
Jul 15, 2024, 4:20:36 AM7/15/24
to material...@googlegroups.com

Dear,

As per ASME the preheating and interpass temperature is 95°C to 120°C.


saleem manhappulath

unread,
Jul 15, 2024, 4:42:59 AM7/15/24
to material...@googlegroups.com
Hi sir

From where did you get this information 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


Prathab P

unread,
Jul 16, 2024, 1:06:07 AM7/16/24
to material...@googlegroups.com

saleem manhappulath

unread,
Jul 16, 2024, 10:05:02 AM7/16/24
to material...@googlegroups.com
Dear Sir,

   So, for the material maximum inter pass temp 315 degree as per API 582, we need to mention 120 degree in the WPS right as per your table which is low 
 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

Prathab P

unread,
Jul 17, 2024, 2:30:21 AM7/17/24
to material...@googlegroups.com
Sir,

The interpass temperature for welding ASTM A572 Gr 50 typically ranges from 150°F to 300°F (65°C to 150°C).

where you get this limits sir?







On Sun, 14 Jul 2024, 23:30 krishnan T, <kris...@gmail.com> wrote:

saleem manhappulath

unread,
Jul 17, 2024, 10:21:47 PM7/17/24
to material...@googlegroups.com
ASTM A572 GR50 is a P1 material . So as per API 582 the inerpass temperature is 315 degree. So kindly check and please update sir

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


Mohamed Ali

unread,
Jul 17, 2024, 11:40:01 PM7/17/24
to material...@googlegroups.com
Dear Saleem 

Yes you are correct , This is P1 Material as per ASME Sec9 and API 582 recommended Interpass temperature for P1 Material 315 Degree Max. 
  
image.png