Hardness - PQR Qualification - Acceptance Criteria for Weld Metal

147 views
Skip to first unread message

Sham Shahabuddin -Welding Inspector, HANBO

unread,
Aug 4, 2022, 5:04:07 AM8/4/22
to material...@googlegroups.com
Dear Experts

Can anyone explain about the Acceptance criteria of Hardness for the weld metal. If my PQR is as per ASME SEC IX and if the hardness test is done, on what basis the test results are acceptable. 

Also please explain the same condition if we are qualifying dissimilar metals

Thanks and Regards 
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING

M.Sathiya Narayanan

unread,
Aug 4, 2022, 7:47:44 AM8/4/22
to material...@googlegroups.com
Hi

Hardness acceptance based on client specification / NACE  applicable also for 
dissimilar metals 





--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6MBwCHpxM0OR-WJoddLhSvug8t6tP3fijAv5Dh-w482bQ%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages