Procedure of Temper Beat Welding

131 views
Skip to first unread message

rao ihsan

unread,
Aug 20, 2013, 10:52:53 AM8/20/13
to material...@googlegroups.com
Dear Expert,
                    I have qualify welders on temper beat welding technique. If some one have procedure for this please share with me

--
Rao Ihsan
Project Engineer

Ph.# +971505702797

james gerald

unread,
Aug 21, 2013, 12:41:18 AM8/21/13
to material...@googlegroups.com
Rao,
 
The attached article will give an idea about Temper  bead welding and help you to prepare a procedure based on the Technique you select.
 
Thanks & Regards


J.Gerald Jayakumar
00968-99438165

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


TGN-PE-02 Temper Bead Welding.pdf

Ramin Kondori

unread,
Aug 21, 2013, 12:36:21 AM8/21/13
to material...@googlegroups.com
Dear Mr. Rao:

Attached please find WTIA's Technical note on temper bead welding (WTIA: Welding Technology Institute of Australia).

Regards
Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.ko...@petroyada.com
+98-2123592322
+98-9132150320



--
Temper Bead Welding (WTIA).pdf