I have welded 25mm PQR using base metal IS2062 E250BR to IS2062 E350C using SMAW. 

Will this qualify Belo combination also;
IS2062 E250BR to Self
IS2062 E350C to Self

or I have to weld two more PQR for above two combination 

Code : Sec IX

Raghuram Bathula

unread,
Mar 15, 2024, 2:06:12 AM3/15/24
to Materials-Welding
Since 350 is unlisted need new qualification, what is the item?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEzKD3J0MTf%2BERKphkz16%2B9QY7K46my3ijAfsPTc7Mn2pt0gwg%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages