we have a wps and pqr for p 43 material of inconel, filler wire
incrmo3.But we can use it for
p45 material uns no n08926? this material grop alloy-622 and filler
wire nicrmo-3 both filler wire is same but gtaw process P number is
assencial as per asme sec 9. i have doubt to use it are not

Raghuram Bathula

unread,
Jan 15, 2011, 3:45:25 AM1/15/11
to Materials & Welding
no, you can't, need separate qualification