Welder Qualified on Plate can weld Pipe?

259 views
Skip to first unread message

sachin sunny N

unread,
Nov 4, 2023, 6:37:46 AM11/4/23
to Materials & Welding
Dear Experts,

Does a welder qualified on plate can do weld on pipe as per ASME? What is the range for that?

mari govindaswamy

unread,
Nov 4, 2023, 8:12:51 AM11/4/23
to material...@googlegroups.com
Plate qualified welder can not weld pipe below 24”, yes he can weld above 24” on pipes 

On Sat, 4 Nov 2023 at 14:37, sachin sunny N <sachins...@gmail.com> wrote:
Dear Experts,

Does a welder qualified on plate can do weld on pipe as per ASME? What is the range for that?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb81cef5-8919-4571-8ada-9222906f059dn%40googlegroups.com.

james gerald

unread,
Nov 4, 2023, 8:12:51 AM11/4/23
to material...@googlegroups.com
Refer ASME Sec.IX   QW-461.9



On Saturday, 4 November, 2023 at 04:07:39 pm IST, sachin sunny N <sachins...@gmail.com> wrote:


Dear Experts,

Does a welder qualified on plate can do weld on pipe as per ASME? What is the range for that?

--

Pradeep Panchal

unread,
Nov 4, 2023, 8:12:51 AM11/4/23
to material...@googlegroups.com
Welder qualified on plate can weld 73mm OD and over. Thickness limit will be 2T of plate qualified.

Regards

Pradeep

On Sat, 4 Nov, 2023, 16:07 sachin sunny N, <sachins...@gmail.com> wrote: