SIMULATED PWHT FOR THE MATERIALS

3,566 views
Skip to first unread message

masthan

unread,
Jun 19, 2010, 2:21:34 PM6/19/10
to material...@googlegroups.com

We are manufacturer of pressure vessels and one of the major client specifications explains about the simulated heat treatment of material as under

 

“Materials with properties enhanced by heat treatment cycles such as tempering, intermediate stress relief (ISR) and the final post weld heat treatment shall be tested to verify that their mechanical properties have been retained after all heat treatment cycles. These tests shall also include two additional post weld heat treatment cycles to account for future repairs or alteration.

 

 

Query: 1: My understanding is that the above paragraph is referring only to the materials for shells & heads of the equipment.

 

Query: 2: My understanding is that the above paragraph is referring only to the material undergoing PWHT in order to achieve certain properties like HIC resistance etc. (or) some specific metals which mechanical properties may enhance due to PWHT not due to thickness for PWHT (ie 38 mm above as per UCS-56).In this case, combined three cycles of SPWHT will fully satisfy the above paragraph requirement.

 

Query: 3: If for the above queries (1 & 2), suppose my understanding is not correct, Please check the below condition for the applicability of Para.

 

For example

·         Dish Head/Toricone of the pressure vessel requires Stress Relieving due to exceeding the allowable fiber elongation as specified in UCS-79(d)

·         Instead of heat treating separate petals of the dish head / toricone, the dish head/toricone petals are welded and also shell portions are welded to it. The complete assembly is then heat treated to relieve residual stresses of Dish head / toricone. (This is done to avoid any distortion caused during Stress relieving of separate petals of the dish head / toricone)

·         In this case, with reference to above Para, whether mechanical properties after one heat treatment cycle need to be tested only for dish head or for all the materials included in the assembly?

 

Please note due to some reason, we are not clarifying the above directly with client. I need opinion from experts.

 

Regards

M.M

Prabhu Kumar L

unread,
Jun 21, 2010, 12:39:57 AM6/21/10
to material...@googlegroups.com

Dear Mr. Masthan,

 

Materials properties enhanced by tempering, means that materials heat treated with Narmalized + Tempered or Quenched + Tempered to retain specific properties (increased toughness with loss in strength) after tempering operation. Also note that these materials if required for PWHT, the PWHT temperature shall be below the tempering temperature in order to retain the properties enhanced by tempering operation. To some extent it will help to reduce HIC cracking problems.

 

You need to ensure the tempering temperature from the material manufacturer and PWHT temperature shall be selected accordingly. As per ASME Sec. IX, QW-407.2, PWHT time at temperature shall be considered as essential variables when impact test is required by other code sections. Hence PWHT cycle time is essential variable, in order to accommodate any repair after PWHT. In general all PQR test coupon shall be required to undergo two to three heat treatment cycle to take care repair.

 

Heat treatment cycle (time at temperature) increases there may a change to reduce the toughness of weld metal since prolonged time at PWHT temperature. At the same time hardness may improve.

 

Regards,

 

L. Prabhu kumar,

Sr. Principal Engineer,

 

Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.





-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or 
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged 
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution 
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If 
you have received this communication in error, please notify us immediately by responding to this email and then 
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete 
transmission of the information contained in this communication nor for any delay in its receipt. 
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

pgoswami

unread,
Jun 21, 2010, 11:16:01 PM6/21/10
to material...@googlegroups.com
Mr. Masthan,
 
Looking at your query it looks to me , you're enquiring about hydroprocessing reactors. Typically modern day reactors are fabricated to ASME SeC-VIII, DIV-2 (for  best design and  best fabricated product)  or SecVIII, DIV-1( as an alternative code).
 
In addition API-934A specifications (Hydrocrackers) and 934C(For Hydro treaters) are also applicable.
 
If you specify the following details:-
  • Design Code, Additional Specifications
  • Materials of constructions
 
then probably the best guidelines could be provided.
 
Both in SecVIII, DIV-1 and DIV-2 codes there are specific requirements for simulated heat treatment and test coupons for steels used for hydroprocessing reactors. In addition the above API Specs outlines how these simulated PWHT is to be perormed and how specimens have to be tested.
 
Thanks.
 
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Ontario Power Generation Inc.
Email-pgoswami@sympatico.ca,
 


Sent: Saturday, June 19, 2010 2:22 PM

To: material...@googlegroups.com
Subject: [MW:5659] SIMULATED PWHT FOR THE MATERIALS
--
Reply all
Reply to author
Forward
0 new messages