Hi,

We have qualified WPS as per ASME SEC IX for material IS 2062 E250 material , now we want to weld material IS2062 E350 material, Can we use the same WPS ?

as IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

Please suggest your views.. Urgent.

--
Thanks and Regards,
Somnath Ashtakar

Charles Jacob

unread,
Mar 19, 2020, 10:25:36 AM3/19/20
to material...@googlegroups.com
Dear, 

If you have qualified a base metal in a particular tensile strength, with a PNo. Then a metal with the same P No but higher tensile is not possible to weld. Your WPS cannot guarantee that weld is safe at higher tensile strengths. 


Hope this helps

Regards, 

Charles V Jacob 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA484EZny6OtkXX518AU1hqCmO9J5gGU69nvMAX%3D-7v8PLfOmA%40mail.gmail.com.

José Juan Jiménez Alejandro

unread,
Mar 20, 2020, 1:05:38 AM3/20/20
to material...@googlegroups.com
IS 2062 E250 - Tensile strength - 410 MPA & 
IS2062 E350 - Tensile strength - 490 MPA

The criterion is not only the Tensile strength, but also the metallurgical similarity, that is the reason why the P Numbers exist, but These materials do not have P Numbers assigned, see Table QW-422.
Saludos!



--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SSI-TPI

Móvil +52 1 812 352 4606

Skype: jjjimeneza





Kannayeram Gnanapandithan

unread,
Mar 20, 2020, 1:05:39 AM3/20/20
to materials-welding
E350 is unassigned. U can not use the same WPS which u are using for E250 which has got assigned Pno 1. Filler material will match E350. 

George Dilintas

unread,
Mar 30, 2020, 1:15:23 AM3/30/20
to material...@googlegroups.com
IS2062 E250 is assigned to P-No1, Grp No 1 (see Non Mandatory App. D of the Section IX)
However, there is no P-No assigned to E350, so  you need a new PQR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA484EZny6OtkXX518AU1hqCmO9J5gGU69nvMAX%3D-7v8PLfOmA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages