SA 541 GR 3 CL 2

150 views
Skip to first unread message

Vishwas Keskar Welding Manager WELDING

unread,
Nov 28, 2023, 12:18:54 PM11/28/23
to Materials & Welding
Experts

Pl. guide for Welding  consumables  compatible for SA 541GR 3 CL 2 pressure vessel plate  butt welding and fillet welding .
Also advice on PWHT time and temperature

Thanks

VISHWAS IWE

james gerald

unread,
Nov 29, 2023, 4:05:56 AM11/29/23
to material...@googlegroups.com
Please try E9018D1 / E9018M

Tempering temperature/SR    :  620degC

Time depends on Applicable code and thickness

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/71bf6501-42f0-43a6-a242-fc1ff3a929adn%40googlegroups.com.

james gerald

unread,
Nov 29, 2023, 4:05:59 AM11/29/23
to material...@googlegroups.com
SA 541 seems to be like Forging