Difference Between IS 2062 Grade A & B

4,750 views
Skip to first unread message

Ravi Karuskar

unread,
May 9, 2011, 6:18:15 AM5/9/11
to material...@googlegroups.com
Dear Experts,

Pls. explain difference between IS 2062 Gr. A & Gr. B.

--
Ravi Karuskar

SARAVANAN C

unread,
May 10, 2011, 7:47:57 AM5/10/11
to material...@googlegroups.com
dear friends,
is2062 gr A and is2062 gr B difference only carbon percetange and
internal bend diameter pls refer is-2062:2006 table-1,2

> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

amje

unread,
May 10, 2011, 8:48:52 AM5/10/11
to material...@googlegroups.com
CARBO PERCENTAGE :GR A -0.23,GRB-0.22,GR C 0.20
WELDABILITY INCREASES FROM A TO C
Y GRROVE CRACKABILITY TEST ONLY FOR GR C.
IMPACT TEST IS NOT DONE FOR GRADE A