ASME B31.3 process piping Hydro in Lieu of RT

310 views
Skip to first unread message

Chaudhary Zafar Iqbal

unread,
Oct 14, 2021, 9:25:33 AM10/14/21
to material...@googlegroups.com
Dear Experts ,
due to time concentrate we are unable to do the RT as we need to arrange the RT crew and ID's process for site access  ...........

as per drawing 5% RT is required .

we can perform hydro of tie in joints ? 

can you please advise for the reference from ASME B31.3  ? 



Best Regards,
Zafar Iqbal 
00966544639978 

Karthik

unread,
Oct 15, 2021, 7:28:28 AM10/15/21
to material...@googlegroups.com
Hi, 
There’s one option in B31.3,- U341.4.1.
A weld coupon examination in accordance with para. U344.8 May be used in lieu of 5% random radiography/ultrasonic examination required in para. 341.4.1(b)(1) when the following  are employed in fabrication.
1. Autogenous automatic welding 
2. Automatic orbital welding with the use of consumable insert rings.

There is no option for hydrostatic in lieu of RT.

Karthik


Sent from Yahoo Mail for iPhone

On Friday, October 15, 2021, 1:13 PM, Karthik <karth...@yahoo.com> wrote:

Hi, 
There’s one option in B31.3,- U241.4.1.
A weld coupon examination in accordance with para. U344.8 May be used in lieu of 5% random radiography/ultrasonic examination required in para. 341.4.1(b)(1) when the following  are employed in fabrication.
1. Autogenous automatic welding 
2. Automatic orbital welding with the use of consumable insert rings.

There is no option for hydrostatic in lieu of RT.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XcM6-QrnGrGm5%3DBN46HRJx_k6DKiaPBs6Pbpjw033JPSA%40mail.gmail.com.

Adnan Ziad

unread,
Oct 15, 2021, 7:28:28 AM10/15/21
to material...@googlegroups.com
tie in must to be radiofraphie or other NDE and its not include in hydro test 
As per Para 345.2.3 (c) of ASME B31.3 you can either do 
100% RT or 100% UT. If Project Specification asks for, you may have to 

--

Chaudhary Zafar Iqbal

unread,
Oct 16, 2021, 3:31:01 AM10/16/21
to material...@googlegroups.com
Dear Respected Members/ experts ,

Greetings 

Thanks for the response from Mr Khatrik and Mr Adnan regarding my previous query .

i would like to ask for the Category D fluid ? what is it ? 

image.png

image.png

as per ASME B31.3 Minimum Temprature is -29 degree centigrade what is maximum temperature is it in asme b31.3 ? .

Fig 323.2.2A
image.png

Karthik

unread,
Oct 16, 2021, 5:45:39 AM10/16/21
to material...@googlegroups.com

james gerald

unread,
Oct 17, 2021, 2:43:09 AM10/17/21
to material...@googlegroups.com
Please see flowsheet for classification of Fluid categories.

Inline image


Thanks & Regards

J.Gerald Jayakumar




Reply all
Reply to author
Forward
0 new messages