Dual certification of material- valve & pipe- SS316/316L ??

427 views
Skip to first unread message

Rana Vikas

unread,
Jul 21, 2010, 7:47:22 AM7/21/10
to material...@googlegroups.com
Dear All,
 
Can you inform meaning of dual grate certification material ??
 
Also send properties of SS316/316L
 
One of our client specification mentioned that piping & valve material should be dual certified i.e SS316/316L .
 
Early reply is appriciable.

Raghuram Bathula

unread,
Jul 21, 2010, 10:58:46 AM7/21/10
to material...@googlegroups.com
simplest way is carbon content as per 316L grade and UTS/YS as per 316 grade will meet both the requirements.

Rana Vikas

unread,
Jul 21, 2010, 11:27:06 AM7/21/10
to material...@googlegroups.com
 
Thanks you.
 
Does mill provide dual certify materials ???

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Raghuram Bathula

unread,
Jul 21, 2010, 11:36:32 AM7/21/10
to material...@googlegroups.com
yes
Reply all
Reply to author
Forward
0 new messages