Flushing & Cleaning Pressure for piping (Applicable code ASME B31.3 )

635 views
Skip to first unread message

Chaudhary Zafar Iqbal

unread,
Oct 21, 2021, 4:32:51 AM10/21/21
to material...@googlegroups.com
Respected Experts ,

Good Day !

Design Pressure :3.5 Bar & Test Pressure as per isometric dwgs : 5.5 Bar 

Test Medium:Water 

operating condition :
Pressure : 0.4 Bar 
Temperature : AMB 

Pipe Size & material  : 6'' A 53 Gr B Seamless 

My Question : is there any restriction in code to limits the test pressure during flushing with water as  our test pressure will be 7 BAR for flushing and also we need to report the same readings in report .

PIPING SYSTEM – FLUSHING AND TESTING


Report No.:

 

Item

Description of Check

Sub Contr.

Contractor

Company

Sign

Date

Sign

Date

Sign

Date

01

Limits of test in accordance with the scope listed on the attached test index and marked-up P&ID’s

 

 

 

 

 

 

02

System prepared for flushing in accordance with the approved procedure.

 

 

 

 

 

 

03

Flushing completed in accordance with the approved procedure

 

 

 

 

 

 

04

System prepared for testing in accordance with the approved procedure

 

 

 

 

 

 

05

System tested in accordance with the approved procedure. (Note 1)

 

 

 

 

 

 

 

Test Results and Readings

Test pressure at start

 

Bar G

Ambient temperature at start

 

oC

Start date and time

 

Date and Time

Test pressure at end

 

Bar G

Ambient temperature at end

 

oC

End date and time

 

Date and Time

Test duration

 

Hours

Tested by contractor

 

Name and Signature

Test witnessed by Company (Note 2)

 

Name and Signature


image.png
image.png


Best Regards,
Zafar 
M:00966544639978

Ramon Briceno

unread,
Oct 21, 2021, 11:11:06 PM10/21/21
to material...@googlegroups.com
Dear Zafar, 

Here my recommendations:
Define the schedule of the pipe, define the length of the span for the flushing, and define the test time. Secure the pipe anchors and supports. Check that it does not generate induced vibration towards static equipment nozzles, as it can generate cracking of the weld.
And most of all, be cautious.

Regards, 
Ramon Briceno 




De: material...@googlegroups.com <material...@googlegroups.com> en nombre de Chaudhary Zafar Iqbal <chzai...@gmail.com>
Enviado: jueves, 21 de octubre de 2021 4:30 a. m.
Para: material...@googlegroups.com <material...@googlegroups.com>
Asunto: [MW:32570] Flushing & Cleaning Pressure for piping (Applicable code ASME B31.3 )
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XcJc%3DZ8C6JrVdk1K1v9iN06t_NeBZrqkfk6OehQ%2BCfdng%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages