Dear All,
We have prequalified WPS of combination GTAW+SMAW
Qualified material :4” Dai X Sch-120(11.02mm)
Garde : ASTM A106 GR B
Welding Process : GTAW +SMAW
Construction Code : ASME SEC IX
Root/ Hot : ER70S-6 Dai 2.4
Fill 1,2 ,3 : E7018 Dai 3.2
Cap : E7018 Dai 2.5.
With Above WPS I would like to extract new WPS for GTAW Process. Please Kindly confirm what shall be the range for GTAW process for parent material thickness . Kindly advice. with reasoning.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEML-XTU9igHwEckWNCH4r_XuWwozo4qRoC_yEXuMvkQrpSuEg%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_fUXMTYF1Ezem7Q_zgt_Rk%3Dmh4R9VwGr9SL7vdH0Mfskw%40mail.gmail.com.
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMBc8CmU4LyyMA8mjrJB9CZDv0ieOtbx_%2BT2GX7jXTrRw%40mail.gmail.com.